Electrode for electrolytic processes such as the recovery of uranium dioxide from seawater comprises an electrically-conductive corrosion-resistant substrate. Coating preferably a mixture of 30 to 80 parts by weight of platinum, 20 to 70 parts by weight (as Mn metal) of,B-Mn02 and 2 to 10 parts by weight. Of tin dioxide.
Electrode for electrolytic processes such as the recovery of uranium dioxide from seawater comprises an electrically-conductive corrosion-resistant substrate. Coating preferably a mixture of 30 to 80 parts by weight of platinum, 20 to 70 parts by weight (as Mn metal) of,B-Mn02 and 2 to 10 parts by weight. Of tin dioxide.
Hak Cipta:
Attribution Non-Commercial (BY-NC)
Format Tersedia
Unduh sebagai PDF, TXT atau baca online dari Scribd
Electrode for electrolytic processes such as the recovery of uranium dioxide from seawater comprises an electrically-conductive corrosion-resistant substrate. Coating preferably a mixture of 30 to 80 parts by weight of platinum, 20 to 70 parts by weight (as Mn metal) of,B-Mn02 and 2 to 10 parts by weight. Of tin dioxide.
Hak Cipta:
Attribution Non-Commercial (BY-NC)
Format Tersedia
Unduh sebagai PDF, TXT atau baca online dari Scribd