Possiblitity Root cause

Current checking method is using visual method. Not using any equipment such as
scope. The burr is to small to be see by naked eye. This method might cause miss
deburring and product leak out.

Transfer Basket

NG Basket OK Basket

Current checking method at NDM

Action Taken
Product need to be sorting using scope because burr is too small. It will be very
difficult for the operator who had eye problems. The small burr must be deburring
using 10X scope SOP manual will be drafted to ensure that the operator in
accordance with the right working procedure.
(Refer SOP Document).

Effective Date: 10/08/16

Reported by:
Wan Syarifuddin
QA Executive
Nakazawa Die Casting(M) Sdn Bhd