DESMODUR® LU-T + MOCA 80 Shore A to 75 Shore D

NATURE OF COMPONENTS CHARACTERISTICS


Prepolymer nature Nature of chain extender and other components Properties
TDI - PTMEG MOCA Amine chain extender - High tensile strength,
- Good abrasion resistance,
- High resilience,
CHARACTERISTICS OF COMPONENTS - Good behaviour at low temperature,
Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® - Good resistance to hydrolysis (water, acid and base) and
Unit LU-T 80 LU-T 90 LU-T 93 LU-T 95 LU-T 60D LU-T 70D LU-T 75D
MOCA
to micro-organisms.
% NCO % 3.2 (± 0.2) 4.2 (± 0.2) 5.2 (± 0.2) 6.1 (± 0.2) 7.3 (± 0.2) 8.5 (± 0.2) 9.2 (± 0.2) - Comments
Physical
appearance at - solid liquid liquid liquid liquid liquid liquid solid - Easy processing (long pot life and low viscosity),
room temperature - Non-toxic material : free TDI content lower than 0.1 %.
Processing Large variety of applications such as industrial rolls,
temperature
°C 80 70 70 70 60 60 60 120
Viscosity at
castors wheels, cushion pads, springs, hydrocyclones,
processing cps 600 900 900 450 750 850 950 - seals…
temperature
Specific gravity at
Others amines available as chain extender (such as
processing - 1.00 1.01 1.02 1.03 1.06 1.09 1.10 1.25 XL 1705 or XL1604)
temperature

ELASTOMER TYPICAL PROPERTIES (DATA GIVEN AS AN INDICATION)


Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur®
Prepolymer
LU-T 80 LU-T 90 LU-T 93 LU-T 95 LU-T 60D LU-T 70D LU-T 75D
Chain extender MOCA MOCA MOCA MOCA MOCA MOCA MOCA
Hardness at 20°C DIN 53505 Shore 80 A 90 A 93 A 95 A 60 D 70 D 75 D
10% Modulus DIN 53504 MPa 2.5 3.9 6 7.9 15.7 32.3 40.8
100% Modulus DIN 53504 MPa 5.0 8.2 12.4 16.5 26.7 40.7 44.2
200% Modulus DIN 53504 MPa 6.5 10.5 16 21.9 34.2 50.9 51.1
300% Modulus DIN 53504 MPa 8.6 13.5 22.9 32.3 45.2 - -
Tensile strength DIN 53504 MPa 23 35 40 45 50 52 54
Elongation DIN 53504 % 510 480 420 360 325 250 230
Tear strength : without nick ISO 34-1 kN/m 69 103 122 144 171 198 205
Tear strength : with nick ISO 34-1 kN/m 22 31 50 57 90 115 120
Resilience DIN 53512 % 55 50 48 42 44 44 45
Abrasion loss ISO 4649 mm³ 35 35 40 45 50 60 75
Compression set (deflection / 22 h / 70 °C) ISO 815-1 % 26 27 28 31 - - -
Hardness at -5°C DIN 53505 Shore 81 A 92 A 94 A 96 A 65 D 76 D 80 D
Hardness at 80°C DIN 53505 Shore 81 A 90 A 92 A 94 A 53 D 58 D 67 D
Specific gravity 1.08 1.08 1.11 1.13 1.16 1.18 1.19
Labelling : This system data sheet is only valid in combination with the corresponding components current safety data sheets ! Any updating of safety relevant information – in accordance with EU directives – will only be reflected in the Safety Data Sheets, copies of which will be revised and
distributed. For further technical information relating to safety, the Safety Data Sheets should be consulted.

BAULÉ - ZI - 46, avenue des Allobroges - BP 116 - 26103 Romans cedex - France - Tel. 33 (0)4 75 72 72 75 - Fax 33 (0)4 75 02 11 73 - E-mail : info@baule.com - www.baule.com
BAULÉ Systems Division is certified ISO 9001 : 2008
Version 12
DESMODUR® LU-T + MOCA 80 Shore A to 75 Shore D

STORAGE AND USE PRECAUTIONS


Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur®
Unit MOCA
LU-T 80 LU-T 90 LU-T 93 LU-T 95 LU-T 60D LU-T 70D LU-T 75D
Optimal storage temperature of the drums °C < 30 < 30 < 30 < 30 < 30 < 30 < 30 < 30
Storage time (sealed drum) Month 6 12 12 12 12 12 12 12
PREPARATION BEFORE PROCESSING
Melting at 110°C
Preheating time / preheating temperature hr / °C 12 / 60 6 / 60 minimum before
use
Homogenization before processing required - no no no no no no no no
Degassing required - yes yes yes yes yes yes yes no

Keep from heat and protect against moisture.

PROCESSING
Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur® Desmodur®
Prepolymer
LU-T 80 LU-T 90 LU-T 93 LU-T 95 LU-T 60D LU-T 70D LU-T 75D
Chain extender MOCA MOCA MOCA MOCA MOCA MOCA MOCA
Hardness Shore 80 A 90 A 93 A 95 A 60 D 70 D 75 D
Prepolymer processing temperature °C 80 70 60
MOCA processing temperature °C 120
Parts by weight of prepolymer 100 100 100 100 100 100 100
Parts by weight of MOCA 9.7 12.7 15.7 18.4 22.0 25.7 27.8
MOLDING AND CURING
Mold temperature °C 100
Pot life (400g mixture) min 18’ 14’ 11’ 6’ 3’30’’ 2’20’’ 1’45’’
Demolding time min 60’ 30’ 30’ 25’ 15’ 15’ 10’
Post-curing hr / °C 16 / 100

Use of degassing agent is recommended for hand casting.


A one week aging at room temperature is required to obtain the optimal properties of the elastomer.

The following information and our technical advice – whether verbal, in writing or by way of trials – are given in good faith but without warranty, and this also applies where proprietary rights of third parties are involved. Our advice does
not release you from the obligation to check its validity and to test our products as to their suitability for the intended processes and uses. The application, use and processing of our products and the products manufactured by you on
the basis of our technical advice are beyond our control and, therefore, entirely your own responsibility. Our advice concerning safety does not release you from the obligation to determine the safety measures designed for your
production environment, that we may not be able to anticipate, to check abilities and to inform the people who will use, handle or be in contact with these products.

BAULÉ - ZI - 46, avenue des Allobroges - BP 116 - 26103 Romans cedex - France - Tel. 33 (0)4 75 72 72 75 - Fax 33 (0)4 75 02 11 73 - E-mail : info@baule.com - www.baule.com
BAULÉ Systems Division is certified ISO 9001 : 2008
Version 12

Anda mungkin juga menyukai