Anda di halaman 1dari 2

XIAMETER® OFS-6020 Silane

Diaminofunctional silane

FEATURES APPLICATIONS
• Coupling agent •
®
XIAMETER OFS-6020 Silane has been found to be an effective
• Improved adhesion coupling agent for clay reinforced elastomers such as natural and
• Increased wet and dry tensile nitrile rubber. The silane-treated clay provides improvement in both
strength and modulus to the physical and dynamic properties compared to similar cured
composite elastomers containing untreated clay.
• Increased wet and dry flexural • XIAMETER OFS-6020 Silane has been reported to be an effective
strength and modulus to the coupling agent for mineral reinforced nylon 6, nylon 6/6 and
composite polybutyleneterephthalate
• Increased wet and dry • Fiberglass reinforced phenolic, melamine and epoxy thermoset
compressive strength composites, either as fiberglass finish or as resinous additive.
• Improved compatibility • As an additive to improve the performance of these types of
between inorganic filler and thermoset resins when they are used as mineral binders in foundry
organic polymer and abrasive composite applications.
• Coupling agent for phenolic, melamine and other organic resins used
as binders for glass and mineral wood insulation, abrasives and
molding components.

TYPICAL PROPERTIES
Specification Writers: These values are not intended for use in preparing
®
specifications. Please contact your local XIAMETER sales representative
prior to writing specifications on this product.

Test Unit Value


Appearance Clear liquid
Flash point – closed cup °C (°F) 85 (185)
Specific Gravity at 25°C (77°F) 1.03
Refractive index 1.445
Neutral equivalents g/eq 115
Color Light straw
Viscosity mm2/s 5

DESCRIPTION of additive should be


XIAMETER OFS-6020 Silane determined by testing several
possesses both organic and concentrations. When used as
inorganic reactivity. XIAMETER an additive to epoxy coatings,
OFS-6020 Silane can react with this product improves adhesion
organic polymers and glass or of the coating, particularly in a
other inorganic mineral very humid environment.
surfaces.
XIAMETER OFS-6020 Silane
HOW TO USE can be applied to inorganic
When used as a resin additive, surfaces, like other silanes, as
generally the silane is added at a dilute aqueous solution (0.1%
a level of less than 1% based to 0.5%) silane concentration).
on the weight of the resin Aqueous solutions can be
solids. For each specific prepared by simply adding the
application, the optimum level silane to water with stirring.
However, poor agitation when PRODUCT SAFETY LIMITED WARRANTY
adding XIAMETER OFS-6020 INFORMATION INFORMATION –
Silane to water can result in PRODUCT SAFETY
locally high concentration which
PLEASE READ
INFORMATION REQUIRED CAREFULLY
may form gel particles. It is FOR SAFE USE IS NOT
normally recommended that the The information contained
INCLUDED IN THIS herein is offered in good faith
silane solution be acidified to a DOCUMENT. BEFORE
pH of 3.0 to 4.5 with an organic and is believed to be accurate.
HANDLING, READ PRODUCT However, because conditions
acid, such as acetic acid, to AND MATERIAL SAFETY
obtain optimum performance of and methods of use of our
DATA SHEETS AND products are beyond our
reinforcing material such as CONTAINER LABELS FOR
fiberglass. control, this information should
SAFE USE, PHYSICAL, not be used in substitution for
ENVIRONMENTAL, AND customer’s tests to ensure that
Inorganic surfaces can be HEALTH HAZARD
treated with the aqueous our products are safe, effective,
INFORMATION. THE and fully satisfactory for the
solution by either dipping or MATERIAL SAFETY DATA
padding. In the case of intended end use. Suggestions
SHEET IS AVAILABLE ON of use shall not be taken as
siliceous mineral fillers, the ®
THE XIAMETER WEB SITE inducements to infringe any
mineral can be treated by AT WWW.XIAMETER.COM.
slurrying in the aqueous patent.
solution or mixed with the
silane at very high shear
STORAGE Dow Corning’s sole warranty is
without any additional solvent. Product should be stored at or that our products will meet the
below 25°C (77°F) in original, sales specifications in effect at
unopened containers. The most the time of shipment.
After applying the silane, the up-to-date shelf life information
glass or mineral surface can be can be found on the Your exclusive remedy for
air dried or dried briefly at 105° XIAMETER Web site in the breach of such warranty is
to 120°C (221° - 248°F) to Product Detail page under limited to refund of purchase
effect complete condensation of Sales Specification. price or replacement of any
silanol groups at the surface product shown to be other than
and to remove water and/or as warranted.
Keep away from heat and open
traces of methanol. Optimum
flame.
application and drying DOW CORNING
conditions, such as time and SPECIFICALLY DISCLAIMS
temperature, should be LIMITATIONS
ANY OTHER EXPRESS OR
determined for each application This product is neither tested
IMPLIED WARRANTY OF
prior to use in a commercial nor represented as suitable for
FITNESS FOR A
process. medical or pharmaceutical
PARTICULAR PURPOSE OR
uses. Not intended for human
MERCHANTABILITY.
injection. Not intended for food
use.
DOW CORNING DISCLAIMS
LIABILITY FOR ANY
INCIDENTAL OR
CONSEQUENTIAL
DAMAGES.

XIAMETER® OFS-6020 Silane 2012, July 28 XIAMETER is a registered trademark of Dow Corning Corporation.
Form No. 95-441B-01 Dow Corning is a registered trademark of Dow Corning Corporation.
©2009 - 2012 Dow Corning Corporation. All rights reserved.

Anda mungkin juga menyukai