SUMBER MATERIAL I. MATERIAL 1. Semen Portland produksi Chonch (Type 1) 2. Aggregat Kasar produksi Stone Crusher EX Telang TANJUNG PINANG 3. Pasir dari Quary EX Pontianak Sungai Mahakam 4. Admixture 5. Air (bebas dari kadar lanau) sumur bor
JMF PROPORSI CAMPURAN BETON 1 M3
NO MUTU BETON SLUMP TEST SEMEN SAK AIR SPLITE PASIR ADIFTIF KET
1 fc 10 12 ± 2 cm 276.12 5.52 161.230 1,158.51 821.14 0.00
2 fc 30 10 ± 2 cm 440.48 8.81 167.280 1,159.24 650.00 0.00
3 fc 25 mpa/fs 3.5 2 - 5 cm 407.93 8.16 179.000 1,025.92 767.15 0.00
4 fc 30 mpa /fs 3.8 2 - 5 cm 458.97 9.18 179.000 2,380.00 716.10 0.00
PROPORSI CAMPURAN BETON DI LAP ( Bachintplong )
NO MUTU BETON SLUMP TEST SEMEN SAK AIR SPLITE PASIR ADIFTIF SEMEN DI LAP
1 fc 10 12 ± 2 cm 276.12 7.00 161.230 1,158.51 821.14 0.00 333.33
2 fc 30 10 ± 2 cm 440.48 11.00 167.280 1,159.24 650.00 0.00 1000
3 fc 25 mpa/fs 3.5 2 - 5 cm 407.93 8.16 179.000 1,025.92 767.15 0.00
4 fc 30 mpa /fs 3.8 2 - 5 cm 458.97 9.18 179.000 2,380.00 716.10 0.00